Kiln Coating
« on: March 19, 2012, 01:21:48 PM »
Does anyone have an opinion about having your kilns coated? I have hears every year, and I have heard every 3-5 years. Some have even went as far to say, it is a waste of money.

What are your thoughts??
Regards,

Francis Bushaw

Offline SenecaMike

  • Newbie
  • *
  • Posts: 8
    • View Profile
Re: Kiln Coating
« Reply #1 on: March 19, 2012, 03:12:19 PM »
Every 2 years works for me as long as the kiln is prepped well before the kiln coat is applied. I make sure the fan shrouds get cleaned off well before application too.

Offline fbushaw

  • Newbie
  • *
  • Posts: 34
    • View Profile
Re: Kiln Coating
« Reply #2 on: March 20, 2012, 10:26:49 AM »
Thanks Mike
I had my 5 kilns coated last year, and it was spendy to say the least!! I am just wondering how great the pay back is from doing every 2 years. I know the old stuff they used to use was very think, and coated eveything very well, it just seems like the stuff they are using now days is a very light coat, almost like spray paint.
Regards,

Francis Bushaw

 


Search


* Forum Experts

MichaelM MichaelM
Forum Expert
TimothyD TimothyD
Forum Expert
PhilM PhilM
Forum Expert
StavrosA StavrosA
Forum Expert

* Subscribe to Newsletter

* Upcoming Events

Sorry! There are no calendar events available at the moment.
\
SimplePortal 2.3.6 © 2008-2014, SimplePortal